View Full Version : My first generator (work in progress)
Argos
09-14-2008, 03:34 PM
Hello.
I new to this. And after unsuccessful buy of my first hho kit from eBay!!!!! I realize that to make it work properly I need to make one myself. This is my first attempt. I have not received my plates yet so did not start on sell (all of my plates are 316 and 3” by 6”).
I need to know if I am on the right track, so any comments, suggestion and remarks well help a lot!!
Thanks.
http://belartllc.com/hho/DSC00549.JPG
http://belartllc.com/hho/DSC00545.JPG
http://belartllc.com/hho/DSC00546.JPG
http://belartllc.com/hho/DSC00547.JPG
hydrotinkerer
09-14-2008, 04:14 PM
I'm not sure why you have two outlets at the bottom of cell? I don't know what kind of electrolite you want to use, But the brass will corrode very fast. My cell had two brass pieces on it and in just a few minutes it corroded. I really like the looks of it, I can't wait to see finished unit. Oh yeah nice floor!:)
EltonBrandd
09-14-2008, 05:08 PM
I have one question, is the floor laminate?
Seriously though, I'm guessing your SS cannister is your negative electrode as well???
Argos
09-14-2008, 06:14 PM
Two outlets at the bottom of cell they are for cooling IN and OUT. If you can see in one of the pictures brass bolts are all coated with epoxy. I hope I don’t get any corrosion from them.
I'm not sure why you have two outlets at the bottom of cell? I don't know what kind of electrolite you want to use, But the brass will corrode very fast. My cell had two brass pieces on it and in just a few minutes it corroded. I really like the looks of it, I can't wait to see finished unit. Oh yeah nice floor!:)
Argos
09-14-2008, 06:22 PM
No. This floor is not laminate. It’s prefinished ¾ hard wood :)
It wasn't in my plans to use canister as negative electrode. But all give it a shot sins I have this option. Thanks for the idea.!!
I have one question, is the floor laminate?
Seriously though, I'm guessing your SS canister is your negative electrode as well???
HHOhoper
09-14-2008, 09:00 PM
I agree with hydrotinkerer. Keep a really close eye on those brass barbs. I've used them too, but they are always out of the electrolyte.
Q-Hack!
09-14-2008, 09:29 PM
Something to keep in mind about those canisters... they are very thin walled. I tried one like it in an earlier experiment. They are also a fairly low grade of stainless steel. Mine was magnetic, you may want to check if yours is.
redneckgearhead34
09-15-2008, 09:13 PM
are you going for a dry cell?